Alloy family
Nickel Alloys: Grades, Composition and Selection Guide
Nickel alloys use nickel as the base (typically Ni ≥ 50%) with Cr, Mo, Cu and Nb additions, outperforming stainless steel in oxidising/reducing media, high temperature and seawater. Hangbo supplies the full Inconel, Hastelloy, Monel and Incoloy range.
Why specify this alloy family
Corrosion resistance
Far superior chloride stress-corrosion-cracking resistance to 300-series stainless
Heat resistance
Most grades serve continuously at 600–1100 °C
Fabrication
Weldable and formable with matched filler metals and procedures
Grades in this family
| Grade | UNS | Density | Tensile | Max service temp. | Detail |
|---|---|---|---|---|---|
| Hastelloy B-2 | N10665 | 9.22 g/cm³ | ≥ 760 MPa | 1000 °C | see Hastelloy B-2 data |
| Hastelloy B-3 | N10675 | 9.22 g/cm³ | ≥ 760 MPa | 1000 °C | see Hastelloy B-3 data |
| Hastelloy C-2000 | N06200 | 8.50 g/cm³ | ≥ 690 MPa | 1040 °C | see Hastelloy C-2000 data |
| Hastelloy C-22 | N06022 | 8.69 g/cm³ | ≥ 690 MPa | 1035 °C | see Hastelloy C-22 data |
| Hastelloy C-276 | N10276 | 8.89 g/cm³ | ≥ 690 MPa | 1040 °C | see Hastelloy C-276 data |
| Hastelloy X | N06002 | 8.22 g/cm³ | ≥ 655 MPa | 1200 °C | see Hastelloy X data |
| Incoloy 800 | N08800 | 7.94 g/cm³ | ≥ 520 MPa | 1100 °C | see Incoloy 800 data |
| Incoloy 800HT | N08811 | 7.94 g/cm³ | ≥ 450 MPa | 1100 °C | see Incoloy 800HT data |
| Incoloy 825 | N08825 | 8.14 g/cm³ | ≥ 586 MPa | 1000 °C | see Incoloy 825 data |
| Incoloy 926 | N08926 | 8.10 g/cm³ | ≥ 650 MPa | 1000 °C | see Incoloy 926 data |
| Incoloy A-286 | S66286 | 7.93 g/cm³ | ≥ 895 MPa (aged) | 700 °C | see Incoloy A-286 data |
| Inconel 600 | N06600 | 8.47 g/cm³ | ≥ 550 MPa | 1095 °C (oxidation resistant) | see Inconel 600 data |
| Inconel 601 | N06601 | 8.11 g/cm³ | ≥ 600 MPa | 1250 °C (oxidation resistant) | see Inconel 601 data |
| Inconel 617 | N06617 | 8.36 g/cm³ | ≥ 655 MPa | 1100 °C | see Inconel 617 data |
| Inconel 625 | N06625 | 8.44 g/cm³ | ≥ 830 MPa | 980 °C | see Inconel 625 data |
| Inconel 690 | N06690 | 8.19 g/cm³ | ≥ 586 MPa | 1000 °C | see Inconel 690 data |
| Inconel 718 | N07718 | 8.19 g/cm³ | ≥ 1275 MPa (aged) | 650 °C | see Inconel 718 data |
| Inconel 725 | N07725 | 8.31 g/cm³ | ≥ 1137 MPa (aged) | 650 °C | see Inconel 725 data |
| Inconel X-750 | N07750 | 8.28 g/cm³ | ≥ 1170 MPa (aged) | 700 °C | see Inconel X-750 data |
| Monel 400 | N04400 | 8.80 g/cm³ | ≥ 480 MPa | 600 °C | see Monel 400 data |
| Monel K-500 | N05500 | 8.44 g/cm³ | ≥ 965 MPa (aged) | 600 °C | see Monel K-500 data |
| Nickel 200 | N02200 | 8.89 g/cm³ | ≥ 380 MPa | 315 °C | see Nickel 200 data |
| Nickel 201 | N02201 | 8.89 g/cm³ | ≥ 345 MPa | 600 °C | see Nickel 201 data |
| Nimonic 75 | N06075 | 8.37 g/cm³ | ≥ 560 MPa (annealed) | 1000 °C | see Nimonic 75 data |
| Nimonic 80A | N07080 | 8.19 g/cm³ | ≥ 1000 MPa (aged) | 815 °C | see Nimonic 80A data |
| Nimonic 90 | N07090 | 8.18 g/cm³ | ≥ 1080 MPa (aged) | 920 °C | see Nimonic 90 data |
Select any grade for full chemical composition, mechanical properties, standards and applications.
Grade data sheets
Hastelloy B-2UNS N10665 · ≥ 760 MPa tensile · 1000 °C maxhastelloy-b-2
Hastelloy B-3UNS N10675 · ≥ 760 MPa tensile · 1000 °C maxhastelloy-b-3
Hastelloy C-2000UNS N06200 · ≥ 690 MPa tensile · 1040 °C maxhastelloy-c-2000
Hastelloy C-22UNS N06022 · ≥ 690 MPa tensile · 1035 °C maxhastelloy-c-22
Hastelloy C-276UNS N10276 · ≥ 690 MPa tensile · 1040 °C maxhastelloy-c-276
Hastelloy XUNS N06002 · ≥ 655 MPa tensile · 1200 °C maxhastelloy-x
Incoloy 800UNS N08800 · ≥ 520 MPa tensile · 1100 °C maxincoloy-800
Incoloy 800HTUNS N08811 · ≥ 450 MPa tensile · 1100 °C maxincoloy-800ht
Incoloy 825UNS N08825 · ≥ 586 MPa tensile · 1000 °C maxincoloy-825
Incoloy 926UNS N08926 · ≥ 650 MPa tensile · 1000 °C maxincoloy-926
Incoloy A-286UNS S66286 · ≥ 895 MPa (aged) tensile · 700 °C maxincoloy-a-286
Inconel 600UNS N06600 · ≥ 550 MPa tensile · 1095 °C (oxidation resistant) maxinconel-600
Inconel 601UNS N06601 · ≥ 600 MPa tensile · 1250 °C (oxidation resistant) maxinconel-601
Inconel 617UNS N06617 · ≥ 655 MPa tensile · 1100 °C maxinconel-617
Inconel 625UNS N06625 · ≥ 830 MPa tensile · 980 °C maxinconel-625
Inconel 690UNS N06690 · ≥ 586 MPa tensile · 1000 °C maxinconel-690
Inconel 718UNS N07718 · ≥ 1275 MPa (aged) tensile · 650 °C maxinconel-718
Inconel 725UNS N07725 · ≥ 1137 MPa (aged) tensile · 650 °C maxinconel-725
Inconel X-750UNS N07750 · ≥ 1170 MPa (aged) tensile · 700 °C maxinconel-x-750
Monel 400UNS N04400 · ≥ 480 MPa tensile · 600 °C maxmonel-400
Monel K-500UNS N05500 · ≥ 965 MPa (aged) tensile · 600 °C maxmonel-k-500
Nickel 200UNS N02200 · ≥ 380 MPa tensile · 315 °C maxnickel-200
Nickel 201UNS N02201 · ≥ 345 MPa tensile · 600 °C maxnickel-201
Nimonic 75UNS N06075 · ≥ 560 MPa (annealed) tensile · 1000 °C maxnimonic-75
Nimonic 80AUNS N07080 · ≥ 1000 MPa (aged) tensile · 815 °C maxnimonic-80a
Nimonic 90UNS N07090 · ≥ 1080 MPa (aged) tensile · 920 °C maxnimonic-90
Available product forms
Round BarsRound Bars
Seamless Tubes & PipesSeamless Tubes & Pipes
Plates & SheetsPlates & Sheets
Precision StripsPrecision Strips
Forgings & RingsForgings & Rings
Welding Wire & CoilsWelding Wire & Coils
Flanges & Pipe FittingsFlanges & Pipe Fittings
Precision Machined PartsPrecision Machined Parts